hey gang.. I also have used garfs method to a degree...
100% portland no aragonite in the mix..
mix it fairly wet, and pour into sand/aragonite shaped mold.. let sit over night to harden. I then soak in water for about an hour or so then let sit out to dry again. my first batch was made in...
hey everyone...
i have a 55g and want to see about cutting the glass on the back of the tank. i know the bottom glass is tempered and cant be drilled out... but what about the back? basically my goal is to have an over flow draining to a refugium/sump...
your thoughts?